Differential Scanning Calorimetry (DSC)
Differential Scanning Calorimetry (DSC)
| MANUFACTURER | TA Instruments |
|---|---|
| MODEL | Q2000 |
General description:
Provide energy variation associated to material phase transition and chemical reaction in a control atmosphere.
Characteristics :
- Temperature modulation capability with amplitude and period selection
- Dual mass flow controllers with gas switching through software control
- Patented Tzero technology provides best sensitivity and resolution baseline
- Photo calorimeter Accessory (PCA) permits characterization of photo curing materials
- Auto Sampler (50 position)
- Temperature range:
- Ambiant to 725˚C (air cooling)
- -90˚C to 550˚C (mechanical cooling)
- -180˚C to 550˚C (liquid nitrogen manual cooling)
- Temperature accuracy: ± 0.1˚C
- Temperature precision: ± 0.01˚C
- Calorimetric Precision: ± 0.05% (based on metal standards)
- Maximum calorimetric sensitivity: 0.2 µW
- Base line curvature (-50˚ to 300˚C): 10µW
- Base line reproducibility: 10µW
- Base line noise (max peak to peak): ≤ 1 µW
- Dynamic range: +/- 500 mW